TECHNET Archives

December 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Ingemar Hernefjord (KC/EMW)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ingemar Hernefjord (KC/EMW)
Date:
Tue, 14 Dec 2004 12:59:36 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (71 lines)
I know, Ofer,

got the content of a 450 V wetolyte in my face when it exploded. But the push-pull power stage with english Williamson transformer (weight about 12 pounds!) and KL66 was worth it. 1965 and 50 W and straight characteristic 20-20 kHz, that was rare for private persons. And homebuilt, twisted exponential stereo horns (about 1 cubic meter each, wife didn't like them). Now I use a 10 band Sony placed in my pocket, and a superlight headset. Times change...

Below, you say that today's caps are 22uF ceramics...hmmmm...why not tantalytes....smells fish..
probably big old pike...

Ingemar


-----Original Message-----
From: Ofer Cohen [mailto:[log in to unmask]]
Sent: den 14 december 2004 09:52
To: TechNet E-Mail Forum; Ingemar Hernefjord (KC/EMW)
Subject: RE: [TN] Dry tantalytes


Ingemar,
Didn't see it since those jolly old days of the wet electrolytes. We used then old, very old, caps over the 250VDC of the tubes anodes to test the technicians nerves... and how well they can smell the results.

Didn't see the problem since then. Keeping x2 ratio between the actually applied voltage and the nominal voltage proves itself. apart of this, we are using ceramic caps up to 22 uF.

Regards
Ofer Cohen
Manager
Quality Assurance, Reliability and Production Technologies
Seabridge Ltd. - A Siemens Company

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ingemar Hernefjord (KC/EMW)
Sent: Tuesday, December 14, 2004 10:21
To: [log in to unmask]
Subject: [TN] Dry tantalytes


The well known epoxy moulded SMT model for P-P is a blessed component when space is limited on the boards. There are several manufacturers, a good uF and VDC range, and we should be happy. But some get trouble from the start. From a population of 1,000 caps, some individuals will pop as soon as voltage is switched on. Remaining caps may work well for thousands of hours. If you study the early life of tantalytes, slow increase of voltage on Curve Tracer, you'll see small transients when the cap is charging. Means minor breakthroughs of the dielectric. After some resting, you can increase voltage again, and also find that the leakage current is quite low and normal, i.e. microamps. The phenomenon is called 'selfhealing' and is well known, not to say the way a tantalyte works. However, if the inrush current is not limited by a suitable series resistance, the energy may overrun the selfhealing capacity, and you'll get a permanent damage. Gives you a unacceptable leakage or even !
 a short, or in worst case, an explosion. Such is the situation. The caps have kind of Akilles heal, and most cap manufacturers tell us as users how to handle the small creeps. E.g. after long storage (not specified) the caps may have to be 'formed' with a kind charging, before they are ready to work. Another example is that you must use a series resistance, say some 1 Ohm/VDC, in order to limit inrush currents, that can damage the dielectric. And derate vs temp, give enough cooling, limit ripple etc... We know all this since years back, but also that many of us as designers do not follow the recommendation, but want to use the full charge/discharge capacity without to much series resistance. The result is that some caps will shorten.

This was the prelude. Maybe slightly in the minor key. Nothing new. What I find remarkable is that you never see a notation on TN about SMT dry tantalytes. One or two exploded caps may not be a trouble in most cases, but for those making HiRel parts, it's not very popular. We speak about 10-30 years life and few events per thousands of operate hours.

The cap manufacturer can feel safe. We don't discuss various brands offically. Instead, I would like to put it like this:

a) are there any more out there with early incident experience (poffs).
b) how do you avoid the problem (screening? series resistors? etc)
c) restricted use of tantalytes

Better suited for SMT forum or IMAPS, but I know there are more of old dogs on TN..myself being over 60....after all, why bother about capacitors...'d better take my Nikon D70, new Sigma 400 and stroll in the forest and focus on living things...sigh..

Ingemar Hernefjord
Ericsson Microwave Systems

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2