See also
http://www.macprintedcircuits.com/sterling.html
Shipley-Ronal also makes an OSP. Their web site says only:
"Ronacoat OSP A thin Imidazole-based organic solderability preservative
Good for multiple thermal excursions and prolonged shelf life."
Timothy Reeves
QA Manager/Process Engineer
ECD Circuit Board Division
13626 S. Freeman Road
Mulino, OR 97042
(800) 228-8198 Fax (503) 829-5482
-----Original Message-----
From: Stephen R. Gregory [mailto:[log in to unmask]]
Sent: Wednesday, August 02, 2000 6:10 AM
Subject: Re: Organic coating
In a message dated 08/02/2000 2:07:27 AM Central Daylight Time,
[log in to unmask] writes:
<< Hello everyone,
Could you help me out with the following request?
I would like to know what kind of protective coating PCB manufacturers are
using to cover the bare copper at the final stage of the manufacturing.
I know about Entek. Are there others?
What is the thickness applied?
Would bare board test will be carried out before or after that coating?
Where can I find information about the composition of the materials
David Banitt President
Exsight Ltd
12 Hamada st.
Tamar Park, Rehovot
POB 4068 Nes Ziona, 70400
Israel
Tel +972 8 9466940
Fax +972 8 9466941
Email [log in to unmask] >>
Hi David!
Go to:
http://www.electrochemicals.com/
They make an OSP called Glicoat SMD. There's also a really good technical
article that will answer all your questions at:
http://www.electrochemicals.com/tech2.htm
There's one more at:
http://www.electrochemicals.com/carhunt.htm
-Steve Gregory-
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|