TECHNET Archives

April 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
Ken Bloomquist <[log in to unmask]>
Date:
Thu, 3 Apr 2008 12:17:40 -0800
MIME-Version:
1.0
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ken Bloomquist <[log in to unmask]>
Parts/Attachments:
text/plain (47 lines)
We do not reflow lead-free here but if you are using no-clean I suppose
there is a remote possibility that some lead contaminated flux could some
how get onto a board. If you clean after reflow you should be getting
everything off the board.

On a more personal note; if we are worried about that amount of lead
contaminating our planet then I think we've gone way beyond what even the EU
Politicians had envisioned.

Heaven help me if my grandchild eats a circuit card from his cell phone that
I reflowed that has a nano-spec of residual flux that may have once upon
it's life evaporated from an 0402 solder joint containing that most
deadliest substance in the amount of 37% lead, oh horrors!

KennyB

-----Original Message-----
From: Joe Macko [mailto:[log in to unmask]] 
Sent: Thursday, April 03, 2008 12:34 PM
To: [log in to unmask]
Subject: [TN] use of the same reflow oven for Pb-free and Sn Pb reflow

Folks,

Question - I believe that it is common practice to use the same forced
convection reflow oven to reflow Pb-free as well as SnPb boards in
today's world but I was wondering if anyone has experienced any issues
doing this as well as what safeguards should be implemented so Pb-free
flux residue deposited within an oven does not contaminate SnPb boards
(e.g. flux build-up in the oven could redeposit onto boards going
through the oven?). thanks again.

Best regards,

-Joe 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2