Ryan,

We use a company called Sipi Metals.  They recycle the PCB's 100%, including
the tab arrays.  They are located in Chigago, IL.  Their phone number is
(800) 621-8013.  There is a metal recycling company in Phoenix, Az. also,
but I can't remember their name.  I am sure there are other metal recycling
companies local to you as well.  By recycling PCB scrap, tubes, reels,
trays, & solder dross we have generated about $12,000/year in income, and
have saved more than $10,000 a year in waste fees.  We also can say we are
an environmentally friendly company, which goes over well with a lot of our
larger customers (Dell, Toshiba, Unisys, Hyundia, Digital Equipment
Corporation, Compaq, etc...).

For tape & reel recycling see website http://www.componenttech.com or call 1
800-881-0780.
For Tube recycling see website http://www.semicycle.org
For solder dross and solder paste recycling contact the Alpha-Fry Group, a
division of AlphaMetals.  They supply waste drums, transportation, and all
of the required manifestation documentation.

Good Luck.

Kathy Palumbo


> -----Original Message-----
> From: Ryan Jennens [SMTP:[log in to unmask]]
> Sent: Thursday, December 10, 1998 10:12 AM
> To:   [log in to unmask]
> Subject:      [TN] Scrap Bare Boards
>
> Mornin' everybody!
>
> Is there a good way to dispose of above subject?  I don't think we can
> just
> pitch 'em 'cause they have lead on the pads.  There has to be somebody
> that
> can grind 'em up or something.  Maybe we could even make a little $?
> Thanks
> all.
>
> Ryan
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2