TECHNET Archives

October 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 5 Oct 2006 11:11:36 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (88 lines)
Hi Gloria! I recommend your conduct two analytical tests if possible: (1)
an FTIR test to try to match the black residue to either your flux or
tinner; (2) SEM test to see if the black residue is comprised of metal
oxides. Have you tested to see if the 270WR and the tinner are compatible
with each other? Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




             Gloria Brown
             <gloriab@BURTONIN
             DUSTRIES.COM>                                              To
             Sent by: TechNet          [log in to unmask]
             <[log in to unmask]>                                          cc

                                                                   Subject
             10/05/2006 08:34          [TN] Solder iron question
             AM


             Please respond to
             gloriab@burtonind
                ustries.com






Good Morning,



I need some information if available.  I am finding on our lead free solder
irons that there is a black substance that is rising up the soldering
shaft.
We are currently using an Aim 270WR flux, SN100C LF Solder, LF tinner,
Solder iron temp is 720, they are WD1 solder irons.



Can anyone give me some information on what this black substance may be?



Thanks



Gloria

phone 906-932-5970  ext. 26

fax  906-932-9822

[log in to unmask]




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2