TECHNET Archives

September 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
David Hillman <[log in to unmask]>
Date:
Mon, 27 Sep 1999 09:03:55 -0500
Content-type:
text/plain; charset=us-ascii
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (79 lines)
Hi Bertrand! Take a look at IPC specification ANSIJ-STD-002A as a starting point
for answers. Also check out Klein Wassink's book "Soldering in Electronics" ISBN
# 0-901150-14-2 for information. Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]





DESSART <[log in to unmask]> on 09/27/99 07:11:54 AM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to
      DESSART <[log in to unmask]>

To:   [log in to unmask]
cc:

Subject:  [TN] component solderability



Hello techneters,

I repeat my previous question about component solderabiliy.
I am looking for some informations about electrical through hole component
(THC) solderability.
Actually, some problems occur when we have to solder a component on a
multilayer printed card. We are faced to the problem when 3 ground layers at
least are connected to the component metalized hole.
Some finite element simulations of the problem have revealed that the following
parameters are very influent:

- Thermal capacity of the component
- Lead material of the component
- Number of connected ground layers to the component hole
- Layers position
- Boundary conditions

I am looking for some reference, specifications and/or test results about it.

Thank you

Bertrand DESSART
Thermal and Mechanical department
ALCATEL ETCA
Charleroi BELGIUM

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2