The magic word is DI. After you remove the majority of the ions from the
water to make it DI it seeks to regain them and will dissolve normal
plumbing and things like water heaters, that is why it is distributed
thorough special plastic piping. I would look to the people that make in
line heaters that have no storage but just heat the water that passes
through and see if they have one suitable for deionized water
> -----Original Message-----
> From: Kenny Bloomquist [SMTP:[log in to unmask]]
> Sent: Tuesday, March 23, 1999 3:37 PM
> To: [log in to unmask]
> Subject: [TN] DI Water Heater
>
> This is a little off subject except we use hot DI for board cleaning.
>
> We are looking for a small, fast recovery DI water heater. It needs to
> keep
> about 20 gallons per hour usage at least 140F to 160F. Everything we've
> seen is very expensive, espically when we say the magic word, DI.
>
> Any leads would be greatly appreciated.
>
>
> Ken Bloomquist
> Sr. Principal Process Engineer
> PRIMEX Aerospace Company
> P.O. Box 97009
> Redmond, WA 98073-9709
> http://www.primextech.com
>
> Ph: 425-885-5000
> FAX: 425-882-5786
> [log in to unmask]
>
> Northcon/99, Board Member
> http://www.northcon.org
>
> Electronics Manufacturers Association (EMA), Vice President
> http://www.ema-wa.org
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|