Genny,

NyoGel 760 reduces connnector insertion force and prevents oxidation.
True that as all greases do, it attracts dust but we do not find that a problem.
What is most important is the reliability of the connection and for that this
special grease (approved for automotive use) its phenomenal.
The USAF did a study on greases for connectors and found the reliability much
improved.  If you'd like a copy I'll try to find it and send it to you.

Regards,
Bob Landman
H&L Instruments, LLC

----- Original Message -----
From: Genny Gibbard
[mailto:[log in to unmask]]
To: [log in to unmask]
Sent: Fri,
16 Apr 2010 12:35:10 -0400
Subject: [TN] Sticky connector pins,
and lubricants


> We build to class 2.  Our products are generally used for network
> infrastructure.  
> Sometimes some of our connectors require a lot of force to mate in
> production, especially as pin counts go up and up, which can cause
> damage if a pin is slightly bent.  Someone suggested using one of
> those
> Deox-it-Gold products.  I have been looking at the datasheets and
> MSDS
> sheets but I am not sure if this could cause issues or leave
> residues
> that could be a problem.  Do any of you have any experience with
> them,
> or have other suggestions for better lubrication of high pin-count
> gold
> plated connectors?
> 
> Thanks once again for your time and experience,
> 
> > Genny 
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security
> System.
> For more information please contact helpdesk at x2960 or
> [log in to unmask] 
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail
> to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> 

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2