Craig:

Check the Technet archives for previous discussions on the use of electrolytic tin as a final
finish.  If memory serves, some work was done to inhibit the growth of tin whiskers through
incorporating controlled amounts of impurities to codeposit with the tin.  Beyond the whisker
issue, plating slivers from fracture of tin overhang caused by etching is another concern.  Some
have attempted to reflow tin, but given the higher melting point what is being gained over
tin/lead alloy?

Don Vischulis

craig sutton wrote:

> ONE CUSTOMER RECENTLY STARTED SPECIFYING 100-300 MICROINCHES OF
> ELECTROPLATED TIN AS A SURFACE FINISH ON SOME NEW PRODUCTION REQUIREMENTS.
> WE DO NOT HAVE THIS PROCESS IN-HOUSE BUT IT CAN BE EASILY INSTALLED.
>
> I HAVE NOT SEEN THIS FINISH ON OTHER SPECIFICATIONS IN THE PAST.  IS THIS A
> VIABLE CHOICE?  ARE THERE ANY PROBLEMS ASSOCIATED WITH PERFORMANCE AT HIGH
> FREQUENCY (6-15 GHZ)?  DOES THIS FINISH EXHIBIT DENDRITE GROWTH?  UNDER
> WHAT CONDITIONS?
>
> THANK YOU FOR YOUR HELP.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2