You are correct in your assumsion. Brazing can be used on a flexprint
whereas you would take the leadframes and using a brazng wedge on a
welder type machine, you would braze the pins/leadframes to the pads
with a third type of metal. I have not seen this requirement for many
years!

Regards - Jim Barry

-----Original Message-----
From: Collins, Graham [mailto:[log in to unmask]]
Sent: Monday, August 23, 1999 3:03 PM
To: [log in to unmask]
Subject: [TN] brazed connector on flexprint


Hi TechNet
Today's question:  A friend outside my company has a RFQ for a job that
calls for connector pins brazed to a flexprint.  He's not sure what this
means.  Is this requirement unusual, and is it different from soldering
the
pins to the flexprint?  I know that brazing is joining two metal
surfaces
with a third, different metal, which could include soldering, but I'm
wondering if something else is meant by this.

regards,

Graham Collins
Process Engineer,
Litton Systems Canada, Atlantic Facility
(902) 873-2000 ext 6215

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask]
or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2