TECHNET Archives

October 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Franklin D Asbell <[log in to unmask]>
Date:
Thu, 3 Oct 2002 15:05:18 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Don Vischulis <[log in to unmask]>
Subject:
From:
Don Vischulis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<000c01c26b03$bb8143c0$0600a8c0@franklin>
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (59 lines)
Franklin,

If you are referring to welding repair ribbons to inner layer circuit
traces, IPC-2012 states that weld repairs are not acceptable without prior
approval by the customer.

I am not aware of any published reliability data.  Perhaps someone else
knows of some studies.

Don Vischulis

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Franklin D Asbell
Sent: Thursday, October 03, 2002 12:39 PM
To: [log in to unmask]
Subject: [TN] Question regarding welds


I'll try sending this for the third time...hmmm...


Was wondering if there are specifications, standards, requirements, etc
regarding the welding of innerlayers???

Is this an acceptable practice? Are there any data on reliability studies
available anywhere?

And any of your personal comments/opinions would be appreciated
also...thanks

Franklin D Asbell

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2