In this case, we only have one board to assemble.
Yvon Hache, Design Engineer
Concept + Inc.
T: 506-863-2467
F: 506-858-4075
[log in to unmask]
www.concept-plus.com
>>> "Alderete, Michael" <[log in to unmask]> 04/28 8:30 pm >>>
Yvon-
Adhesive backed polyimide tape comes to mind. Polyimide is a high Tg
material, with a very high dielectric breakdown voltage rating. Automating
the application of PI tape might not be so easy, unless some TechNetter has
a particular solution in mind.
Michael Alderete
Yvon Hache wrote...
------------------------------
Date: Wed, 28 Apr 1999 15:00:37 -0300
From: Yvon Hache <[log in to unmask]>
Subject: Isolator
Hello everyone,
I was happy that the snow was all gone on the ground until it start =
snowing about an hour ago. It never ends.
Now the serious stuff.
We are assembling a PCB for a client and there are traces running under a =
transformer on the PCB top side. The metal transformer mounting and these =
traces are only isolated by the soldermask. Is there some kind of =
isolator we can insert between the transformer and the PCB? The voltage =
used on this board is 230Vac, 50Hz.
Thanks
Yvon Hache, Design Engineer
Concept + Inc.
T: 506-863-2467
F: 506-858-4075
[log in to unmask]
www.concept-plus.com
------------------------------
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|