TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Ingemar Hernefjord (KC/EMW)" <[log in to unmask]>
Date:
Thu, 14 Sep 2006 09:41:52 +0300
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
Reuven ROKAH <[log in to unmask]>
X-cc:
In-Reply-To:
MIME-Version:
1.0
Parts/Attachments:
text/plain (104 lines)
Gold over Nickel is a problematic plating for press fit.

The Nickel have a tendency to crack.


Best  Regards

Reuven  ROKAH

e mail: [log in to unmask]



             "Ingemar
             Hernefjord
             (KC/EMW)"                                                  To
             <ingemar.hernefjo         [log in to unmask]
             [log in to unmask]>                                           cc
             Sent by: TechNet
             <[log in to unmask]>                                     Subject
                                       Re: [TN] Press Fitting Soldered
                                       Contacts Into ENIG
             14/09/2006 09:36


             Please respond to
              TechNet E-Mail
                   Forum
             <[log in to unmask]>
             ; Please respond
                    to
                 "Ingemar
                Hernefjord
                 (KC/EMW)"
             <ingemar.hernefjo
             [log in to unmask]>






Brian,
We have a simple rule here: gold-gold or tin-tin (not the cartoon one).
So, never a gold pin into a tinned board or vice versa.
Inge

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: den 12 september 2006 17:24
To: [log in to unmask]
Subject: [TN] Press Fitting Soldered Contacts Into ENIG


Good morning all,
      Are there any particular reliability concerns when press-fitting a
soldered contact (SN63) into a plated barrel with an ENIG surface? What
might the outcome of this be over the long term? Is this an accepted
practice? Would this be acceptable in a class 3 military application?

Thank you for your input.

Brian Guidi
Senior Product Engineer
Teledyne Printed Circuit Technology
Tel: (603) 889-6191  X:310
Fax: (603) 886-2977
E-mail: [log in to unmask]

Visit us @ http://www.tetpct.com

Any technical information attached to this document is intended for the
recipient only.  Also, the export and use of the information is
regulated by the export laws of the United States.  Diversion contrary
to U.S. law is prohibited.  U.S. law prohibits sharing this information
with any end-user for any end-use related to the design, development,
production, stockpiling or use of chemical, biological or nuclear
weapons or missiles, without the prior approval of the United States
Government.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2