Fellow Technetters:
I had been measuring solder thickness on QFPs and found out that the
thickness on horizontal pads is slightly thicker than the vertical pads. I
know this is normal specially for a Vertical Hot Air solder leveler. But
what should be the limit? Also along with test, using an x-ray coating
thickness measuring machine, is it normal that the tin % composition on the
vertical pads lower than horizontal pads? I tried lowering the air knife
pressure thinking that high temperature depletes Sn, but I got similar data
on 200, 210, 220, 230 and 240 C air knife spray pressure.
Garret Dimaculangan
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|