Are there any outfits out there who have engineered their waste streams
to produce salable copper salts?

I am not referring to electrowinning or sludge reclamation but full
scale custom synthesis to minimize wasted copper.
Take the reclamation of copper sufate, synthesis of malachite, or other
copper salts with different gegenions.

Are there any sources of funding to initiate such a project?  Does
anyone see any potential buyers?

One could view one board shop as a remote source for material; but the
collective of shops could be a major source.

Thank you,
One Overactive, Curious Chemist

[log in to unmask] 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2