This is a little driver looking on cloud in the sky...
More seriously- I believe this is oxidised copper below soldermask.Seems to
be harmless, probably visual effect.Usually oxidation on copper does not
effect adhesion.
Edward
> -----Original Message-----
> From: Stephen Gregory [SMTP:[log in to unmask]]
> Sent: ב דצמבר 05 2005 16:49
> To: [log in to unmask]
> Subject: Re: [TN] What is this solder mask defect?
>
> Good Morning Everyone!
>
> I got Wee Mei's picture up...go to:
>
> http://stevezeva.homestead.com/files/Soldermask_Defect.JPG
>
> I've seen this before, but I can't explain it either.
>
> Kind Regards,
>
> -Steve Gregory-
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Wee Mei
> Sent: Sunday, December 04, 2005 6:58 PM
> To: [log in to unmask]
> Subject: [TN] What is this solder mask defect?
>
> Steve,
>
> Hello,
>
> The suspect is completely flat and smooth to touch. An interesting
> observation is that though it appear at the same location for all the
> 10pcs
> of board, the size of the image tend to get smaller and smaller if the
> boards are arranged starting with the largest image. It can't be soda
> strawing as it is not on trace. It can't be pink ring as it is not
> around
> hole. What can it be? What is the likely cause?
>
> Will ask Steve to put it up. Kindly take a look. Your opinion is greatly
> appreciated.
>
> Regards,
> Wee Mei
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|