TECHNET Archives

February 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
Old-Return-Path:
Date:
Wed, 26 Feb 97 14:56:24 PST
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/10714
TO:
Return-Path:
<TechNet-request>
X-Loop:
Resent-Message-ID:
<"6NLcW3.0.AXF.MaD5p"@ipc>
Subject:
From:
<[log in to unmask]> (Vernon Pursley)
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vztyB-0007zYC; Wed, 26 Feb 97 18:45 CST
X-Priority:
3 (Normal)
From [log in to unmask] Thu Feb 27 09:
29:52 1997
Message-Id:
Parts/Attachments:
text/plain (74 lines)
Hi Mike,

This came across IPC Technet.

At lease we are CATCHING the high resistant shorts before shipping them to the 
customer!

Vern

[log in to unmask] Wrote:
| 
|  Good morning Techneters,
|      
|  We have been finding defective PWBs from time to time.  
| The defect 
|  rate is not alarming all the time, however it seems like 
| there is a 
|  small number of defective PWBs are coming in (steadily) 
| with various 
|  defects, such as, open or high resistant via, open trace, 
| poor 
|  solderability, etc.
|      
|  My question to you is, "Is there some percentage that is 
| typical for 
|  escaping defects out of a fab house?"  I know ideally it 
| should be 
|  zero.  What is your experience?
|      
|  Thanks in advance,
|  Paresh Patel
|  Mfg. Engr.
|  Oneac Corp.
|  847-816-6000 x-704.
| 
| **********************************************************
| *****************
| * TechNet mail list is provided as a service by IPC using 
| SmartList v3.05 *
| **********************************************************
| *****************
| * To subscribe/unsubscribe send a message <to: 
| [log in to unmask]>   *
| * with <subject: subscribe/unsubscribe> and no text in the 
| body.          *
| **********************************************************
| *****************
| * If you are having a problem with the IPC TechNet forum 
| please contact   *
| * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at 
| [log in to unmask]      *
| **********************************************************
| *****************
| 
| 


Vern Pursley, Applications Engineering
Merix Corporation
Phone: 503-992-4404;FAX 503-359-2651;
[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2