The "Printed Circuits Handbook" 4th ed. by Clyde F. Coombs Jr. will
not only explain plating but also just about every aspect you can
think of relating to PCB manufacturing. It's available from McGraw
Hill Pub. ISBN 0-07-012754-9
DNHJR
______________________________ Reply Separator _________________________________
Subject: copper plating
Author: [log in to unmask] at corp
Date: 3/25/97 10:32 AM
I am a graduate student working with sequential built-up pcb
technology. We have a plating line in our lab. I want some
publications (e.g. a handbook) related to copper plating (electro) at
hand.
Does anyone there have any information about this?
Thanks in advance.
Suixin from IMEC in Belgium.
suixin zhang
ELIS-TFCG/IMEC, University of Gent
Sint-Pietersnieuwstraat 41, B-9000 Gent, Belgium
tel: 0032-9-2643371
fax: 0032-9-2643594
Email: [log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************