You guys are right on target here. We have a major customer who is world
leader in the heavy vehicle industry, and they were (and I think still
are) very skeptical of our no-clean process (we also use Multicore paste).
We have taken great strides to convince the customer that the no-clean
process meets all industry specifications, and we have set up process
controls to prove it. We hired a very high ranking consultant to set us
on the right track with our customer. The consultant strongly advises
against cleaning the "no-clean" flux. The alternative, to do the job
correctly, would have been a $250,000 investment for a cleaning system.
Howard Watson
Lou Hart <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
02/20/01 09:09 AM
Please respond to "TechNet E-Mail Forum."; Please respond to Lou Hart
To: [log in to unmask]
cc:
Subject: Re: [TN] Washing of no-clean
I was hoping someone would say what Brian has here, on behalf of
manufacturers. If you want something more than conformance to our
standard, 610 class 2 product, tell us you want it up front and be
prepared
to pay for it. This business is not a philanthropic enterprise. It may
be
advisable to give some free advice in this area, however, by telling the
customer he may be wasting his money.
Lou Hart
-----Original Message-----
From: Brian Ellis [SMTP:[log in to unmask]]
Sent: Tuesday, February 20, 2001 9:21 AM
To: [log in to unmask]
Subject: Re: [TN] Washing of no-clean
Ioan
Well, if they want it clean, they will have to pay for it, n'est-ce-pas?
If they don't want to pay, the corollary is that they should put up with
the minimal residues from a good low-solids, "no-clean" flux/paste.
If you buy a car and want to enhance its appearance with "speed-stripes"
or a spoiler, do you think your supplier will do it for free?
Brian
"Tempea, Ioan" wrote:
>
> Sorry for the missing details.
>
> The product is regular office equipment, so not a demanding one. The
request
> for cleanliness is purely aesthetical.
>
> By the way, no premium involved. They want it clean and that's it.
>
> Regards,
> Ioan
>
> > -----Original Message-----
> > From: Brian Ellis [SMTP:[log in to unmask]]
> > Sent: Tuesday, February 20, 2001 2:31 AM
> > To: TechNet E-Mail Forum.; Tempea, Ioan
> > Subject: Re: [TN] Washing of no-clean
> >
> > Ioan
> >
> > Whoa! Be careful here. If your clients are wanting cleaning, there is
a
> > reason why they are willing to pay a premium. What is it? If it is
> > purely for aesthetics, then no great deal. If it is for technical
> > reasons, what degree of cleanliness is required? What is the end-use
> > application? If it is critical, then you must do the job properly and
it
> > would be unlikely a bench-top system would give adequate results, at
> > least without multiple stages and excellent process control.
> >
> > Please let us know more.
> >
> > Brian
> >
> > "Tempea, Ioan" wrote:
> > >
> > > Hi technos,
> > >
> > > I need your expertise again.
> > >
> > > We are on no-clean and newer clients ask us to clean the residue. I
need
> > to
> > > know if any equipment exists to do this job, except for the big
washers.
> > I'm
> > > thinking of a small (table top) tank, followed by some drying thing.
> > > Then, is the simple dipping of the board enough to wash away the
> > residue, or
> > > some agitating action is needed?
> > >
> > > We are on X33 flux from Multicore and I think I can get from them
the
> > right
> > > substance that would do the cleaning. However, if you happen to have
> > > suggestions...
> > >
> > > Thank you,
> > > Ioan
> > >
> > >
> >
--------------------------------------------------------------------------
> > -------
> > > Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
> > > To unsubscribe, send a message to [log in to unmask] with following
text
> > in
> > > the BODY (NOT the subject field): SIGNOFF Technet
> > > To temporarily halt delivery of Technet send the following message:
SET
> > Technet NOMAIL
> > > Search previous postings at: www.ipc.org > On-Line Resources &
Databases
> > > E-mail Archives
> > > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> > additional
> > > information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
> > ext.5315
> > >
> >
--------------------------------------------------------------------------
> > -------
>
>
------------------------------------------------------------------------
---------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
>
------------------------------------------------------------------------
---------
------------------------------------------------------------------------
---------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
---------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
|