I did just this with some standard FR-4 boards, and the lead-free
flipchips soldered up just fine. But at 235 Deg. C. some of the boards
delaminated in spite of a 24 hour bake just prior to assembly and
reflow.
We went to a different circuit board material from North Texas Circuits
(NT) and then they worked perfectly.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phillip Bavaro
Sent: Friday, November 11, 2005 12:15 PM
To: [log in to unmask]
Subject: Re: [TN] Lead Free BGA rework
Hi Gus,
Sure, it can be done but that is a lot of work when you could just use
the lead free BGA as is and raise your reflow profile to 230-235? Sure,
it does raise the question whether or not the other parts on the board
can handle the slightly higher reflow condition, but this intermediate
process has been used quite a bit already.
Hope this helps,
Phil
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|