TECHNET Archives

August 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jean-Luc Lehmann <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 15 Aug 2001 11:28:43 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (61 lines)
I have seen such problem on SMD component with silver-palladium terminal.
These were first intended to be used in hybrid  and assembled by conductive
glue, however we ended up using with reflow soldering and we had occurences
of "broken" terminal connection (the contact was not there anymore and the
part would eventually come loose (without its terminals).  The cause is
that the silver-palladium leach into the solder paste during the reflow
process at high temperature. The cure was to switch to tinned terminals.
If you really need to use these parts them you should try to use solder
with a small amount of silver wich will somewhat prevent leaching.

Jean-Luc Lehmann




                    "Marsico, James"
                    <James.Marsico@D        To:     [log in to unmask]
                    P.AIL.COM>              cc:
                    Sent by: TechNet        Subject:     [TN] Soldering to palladium silver
                    <[log in to unmask]
                    >


                    13.08.01 12:56
                    Please respond
                    to "TechNet
                    E-Mail Forum.";
                    Please respond
                    to "Marsico,
                    James"





Has anyone come across any process or reliability issues when soldering
chip
capacitors with a palladium silver finish without pretinning first?  We
have
a customer who put us on stop work because they have an issue with this.
Any info will be appreciated.

Thanks in advance,

Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2