Mark Hargreaves <[log in to unmask]>
Date:
Mon, 21 Mar 2005 14:18:53 -0500
MIME-Version:
1.0
X-To:
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Mark Hargreaves <[log in to unmask]>
Parts/Attachments:
text/plain (159 lines)
Afternoon All,
Isn't the Tg requirement design driven?  Why not spec as a "minimum"
(dictated by the design) to allow the most flexibility to the fabbers?
MarkH


        -----Original Message-----
        From:   James Hofer [SMTP:[log in to unmask]]
        Sent:   Monday, March 21, 2005 1:40 PM
        To:     [log in to unmask]
        Subject:        Re: [TN] Most common version of FR4?

        Most of our thick core laminates are high Tg due to the industry
moving away
        from low Tg products.
        Our off-shore partners use only high Tg and High Td lead free
laminates as
        is the case with 'most' off-shore manufacturers.
        I see no problem calling out a higher Tg material for double-sided
parts.

        Just my $0.02

        James Hofer
        Director of Operations
        Accurate Circuit Engineering
        3019 S. Kilson Dr.
        Santa Ana Ca. 92707-4202
        714-546-2162 work
        714-473-6127 cell
        [log in to unmask]
        ----- Original Message -----
        From: "Jeffrey Bush" <[log in to unmask]>
        To: <[log in to unmask]>
        Sent: Monday, March 21, 2005 6:52 AM
        Subject: Re: [TN] Most common version of FR4?


        4101/24-26 material is fine for multilayer PCB and is readily
available.
        When looking at materials over .028" in thickness the /24-26
materials
        become special order and are fairly costly.  Much of the
manufacturing
        for rigid laminates has moved off-shore and this also makes it more
        difficult to procure thicker materials in higher Tg epoxies.

        Double Sided boards should be 4101/21 materials unless .028" and
        thinner.

        Jeffrey Bush
        Director, Quality Assurance and Technical Support

        VERMONT CIRCUITS INCORPORATED
          76 Technology Drive - POB 1890
            Brattleboro, Vermont 05302
              Voice: 802.257.4571.21 Fax: 802.257.0011
                   http://www.vtcircuits.com

        -----Original Message-----
        From: Brooks,Bill [mailto:[log in to unmask]]
        Sent: Friday, March 18, 2005 8:59 PM
        To: [log in to unmask]
        Subject: [TN] Most common version of FR4?

        I'm looking for a reading on the most common version of FR4 material
for
        2
        sided boards and for multilayer boards... based upon usage in the
board
        manufacturers shops...

        I want to specify per IPC-4101/??

        The best choices would have better Tg characteristics... so I was
        leaning
        toward IPC-4101/26 as my choice but there may be a suitable
alternative
        that
        is more commonly used that someone can point me to.

        I have some old board designs that were originally build back when
        MIL-P-13949 was the spec and GFN FR4 was all we had to specify...

        It's time to update the notes...
        Any help appreciated... :)

        Best regards,

        Bill Brooks - KG6VVP
        PCB Design Engineer , C.I.D.+, C.I.I.
        Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
        e-mail:[log in to unmask]
        http://www.dtwc.com
        http://pcbwizards.com

        ---------------------------------------------------
        Technet Mail List provided as a service by IPC using LISTSERV 1.8e
        To unsubscribe, send a message to [log in to unmask] with following
text
        in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt or (re-start) delivery of Technet send e-mail to
        [log in to unmask]: SET Technet NOMAIL or (MAIL)
        To receive ONE mailing per day of all the posts: send e-mail to
        [log in to unmask]: SET Technet Digest
        Search the archives of previous posts at:
        http://listserv.ipc.org/archives
        Please visit IPC web site
        http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
        ext.2815
        -----------------------------------------------------

        ---------------------------------------------------
        Technet Mail List provided as a service by IPC using LISTSERV 1.8e
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt or (re-start) delivery of Technet send e-mail to
        [log in to unmask]: SET Technet NOMAIL or (MAIL)
        To receive ONE mailing per day of all the posts: send e-mail to
        [log in to unmask]: SET Technet Digest
        Search the archives of previous posts at:
http://listserv.ipc.org/archives
        Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
        for additional information, or contact Keach Sasamori at
[log in to unmask] or
        847-615-7100 ext.2815
        -----------------------------------------------------

        ---------------------------------------------------
        Technet Mail List provided as a service by IPC using LISTSERV 1.8e
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
        To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
        Search the archives of previous posts at:
http://listserv.ipc.org/archives
        Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
        -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2