TECHNET Archives

October 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 30 Oct 2003 07:53:13 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset="us-ascii"
Subject:
From:
Doug Pauls <[log in to unmask]>
X-cc:
MIME-Version:
1.0
Parts/Attachments:
text/plain (25 lines)
Guy,
The B36 board is divided into four quandrants.  The SMT mounting pads in
quadrants C and D comprise two of the ten SIR test patterns on the board.
These mounting pads are interdigitated, or alternate between the applied
voltage and ground.  You are measuring the SIR between alternating pads.
The intent of these test patterns was to test for solder paste residues.
If you have a component with a blown chip inside, if there is anywhere in
the wire bonding where and even number pad and an odd number pad are
shorted, or if the die itself represents a low resistance path, then the
readings for these two test patterns will be false and often compromise
failures.  The mounting pads in quadrants A and B are not interdigitated,
so it makes no difference what you put in those quandrants.

Doug Pauls

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2