TECHNET Archives

July 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Thayer, Wayne - IIW" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Thayer, Wayne - IIW
Date:
Wed, 21 Jul 2010 09:18:07 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (444 lines)
Hi Werner-

You may recall I brought this issue up a few months ago too.  The basic question I have is

If solder joint height is important for longevity/reliability, why aren't there IPC guidelines/requirements for them?  As noted previously, tungsten rods are available in almost any diameter and they can be used as a simple "quick check" tool for this application.

Wayne

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Tuesday, July 20, 2010 1:01 PM
To: [log in to unmask]
Subject: Re: [TN] solder joint height

 )Dale,
The answer is a qualified YES.
What are the sizes of these ceramic chip components and the Alloy-42-dominated SOT? When do you see those cracks [thermal history]? What are the QUAL requirements?
What is the real use environment?
I take it this is SnPb solder.
Regardless of these answers, a greater SJ height enhances reliability-you may want to take a look at the attached reliability article (Engelmaier,W., "Achieving Solder Joint Reliability in a Lead-Free World, Part 1," GlobalSMT & Packaging, Vol. 7, No. 6, June 2007, pp. 40-42).  .


 Werner






-----Original Message-----
From: Hart, Dale L CTR USAF AFMC AFRL/RXSA <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, Jul 20, 2010 12:51 pm
Subject: Re: [TN] solder joint height


Air Force often uses CCA's as circuit card assemblies, sorry for the confusion.

The type of components are surface mount resistors, capacitor and I believe a

SOT with gull wing leads.



My problem is do I suggest their solder joint height isn't sufficient enough to

ensure a reliable assembly on an aircraft.





dlh



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier

Sent: Tuesday, July 20, 2010 11:19 AM

To: [log in to unmask]

Subject: Re: [TN] solder joint height





 Hi Dale,

Do you mean CGA's [column grid arrays]? If not, what do you mean by cca?



 610, Class 3 or otherwise, only addresses quality, not reliability-for that you

need to go to IPC-D-279.



While the absence of solder fillets can reduce fatigue life, the presence of

fillets, 'robust' or otherwise, does not have any positive first-order impact.

However, solder joint height does.





 You may be looking at IMC crystals.

Werner







-----Original Message-----

From: Hart, Dale L CTR USAF AFMC AFRL/RXSA <[log in to unmask]>

To: [log in to unmask]

Sent: Tue, Jul 20, 2010 9:23 am

Subject: [TN] solder joint height













We have been doing a some analysis of cca's for the Air Force consisting of



SMT.  The visual inspection of the solder joints looks very good all



characteristics above the suggest minimum for class 3 of 610.  The solder



fillets in some instances could be characterized as being robust.  In



cross-sectional analysis however, the solder joint height of the components



electrical termination above the land has been perhaps 0.025 mm to the point



of needing a SEM to look at the land-solder-component lead interface.



Closer examination in these areas revealed small cracks in the grain



boundaries.  I used the term grain boundaries because the solder in these



areas do not resemble the colonies observed in the bulk solder of the



fillet.  In some of these instances the land is often deformed in the shape



of the component lead.















Would these joints although stronger be more susceptible to fatigue or



overload failure?







What are the implications if these cca's are encapsulated?







What suggestions could be offered to the manufacturer?























Dale L. Hart







Universal Technology Corporation (UTC)







Failure Analysis







1270 North Fairfield Road







Dayton, Ohio  45432-2600







(937) 656-9165







Fax (937) 656-4600







Email:  <mailto:[log in to unmask]> [log in to unmask]



















---------------------------------------------------



Technet Mail List provided as a service by IPC using LISTSERV 15.0



To unsubscribe, send a message to [log in to unmask] with following text in



the BODY (NOT the subject field): SIGNOFF Technet



To temporarily halt or (re-start) delivery of Technet send e-mail to



[log in to unmask]: SET Technet NOMAIL or (MAIL)



To receive ONE mailing per day of all the posts: send e-mail to



[log in to unmask]: SET Technet Digest



Search the archives of previous posts at: http://listserv.ipc.org/archives



Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for



additional information, or contact Keach Sasamori at [log in to unmask] or



847-615-7100 ext.2815



-----------------------------------------------------









______________________________________________________________________

This email has been scanned by the MessageLabs Email Security System.

For more information please contact helpdesk at x2960 or [log in to unmask]

______________________________________________________________________



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------



______________________________________________________________________

This email has been scanned by the MessageLabs Email Security System.

For more information please contact helpdesk at x2960 or [log in to unmask]

______________________________________________________________________




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender.
Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2