Sender: |
|
X-To: |
|
Date: |
Thu, 7 Sep 2000 08:20:27 EDT |
Reply-To: |
|
Subject: |
|
MIME-Version: |
1.0 |
Content-Transfer-Encoding: |
7bit |
Content-Type: |
text/plain; charset="US-ASCII" |
From: |
|
Parts/Attachments: |
|
|
In a message dated 09/07/2000 3:47:57 AM US Eastern Standard Time,
[log in to unmask] writes:
>
> With respect to SIR and Electromigration testing, can anyone please
> enlighten me about the two Bellcore standards that are often quoted by flux
> manufacturers. Some datasheets I see quote Bellcore TR-NWT-000078 Issue 3
> and some Bellcore GR-78-CORE. The test conditions look quite similar. Has
> one standard superseded the other or are they both current?
The TR-78 document was superceded in September 1997 by the GR-78 document.
The SIR test is essentially the same between the two documents. The
electromigration test changed from 596 hours at 85C/85% RH in the TR-78 spec
to 596 hours at 65C/85% RH in the GR-78 spec, with the pass-fail criteria
remaining the same.
If the paste or flux passed TR-78 SIR, then it passed GR-78 SIR, although the
manufacturer *should* have had it tested to GR-78 and updated their data
sheets by now.
>
> Ultimately, which is the most suitable for todays Telecomms applications?
Define suitable. Using the classical thinking of a present standard
superceding an outdated standard, the GR-78-CORE document would be "suitable".
>
> Looking forward to your responses.
Must be a slow day for you.........
Doug Pauls
Technical Director
CSL
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|