Technos,
There are 2 main ideas I can gather from your answers:
1. Why do I bother with laser when I could reflow? Well, as I said, reflow seems to warp either the component or the PCB and having no idea about laser soldering myself, I thought it would be a good idea to inquire. Since it seems to have no benefit, I believe I better get back to reflow. But not before asking another one: the BGA is soldered onto flex that is backed by a 12 mil rigid something; are there lasers that could solder from the bottom, through the substrate, rather than through the part, thus minimizing the heat seen by the assembly?
2. Steve K, could you please elaborate regarding the metal stiffener vs. FR-4. To my surprise, it seems that brass stiffeners yield better results than FR-4 indeed; shouldn't they give a bigger CTE mismatch?
Thanks,
Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
T | 450.967.7100 ext.244
E | [log in to unmask]
W | www.digico.cc
N'imprimer que si nécessaire - Print only if you must
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|