TECHNET Archives

July 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Roger Mack <[log in to unmask]>
Date:
Tue, 19 Jul 2005 16:41:10 -0500
MIME-Version:
1.0
X-To:
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Roger Mack <[log in to unmask]>
Parts/Attachments:
text/plain (30 lines)
what procedures are being used to verify adhesion of conformal coating over
no-clean solder paste?    We use a moisture cure silicone. A few years ago
we had three of the major solder paste manufacturers perform SIR tests and
coating adhesion tests.  Most tests referenced the ASTM-3359 which describes
cutting a cross hatch pattern in the coating and performing a tape peel
test. This procedure also has a classification ranking for the results.  We
found that only one of the labs followed this procedure and the others had
either modified or developed a different test since silicone coating is
difficult to apply tape to. There was no issues with the acrylic coatings
tested.  Two of the three labs used the IPC-B-24 test boards.

What proccess is a fair test for silicone coating adhesion?    If ASTM-3359
is used what tape brand meets the specifications given.







---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2