TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Inge <[log in to unmask]>
Date:
Thu, 31 Jul 2008 15:48:21 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (131 lines)
Leland, forgot to tell you that not all resistor chips are for uwave 
applications.
there ARE chips intended for mounting with resistor print against the board, 
e.g.

http://www.caddock.com/Online_catalog/Mrktg_Lit/TypeCHR.pdf

Inge


----- Original Message ----- 
From: "Inge" <[log in to unmask]>
To: "TechNet E-Mail Forum" <[log in to unmask]>; "Leland Woodall" 
<[log in to unmask]>
Sent: Thursday, July 31, 2008 3:28 PM
Subject: Re: [TN] Repair Need for Inverted Chip Resistors


> There are two or three reasons not to turn them up and down (if you are a 
> microwave guy >1 GHz ):
>
> 1. The L-cut laser trim groove may be filled by active substances from the 
> flux. (no glass or paint overprint)
> 2. We have done simulations which show that your insertion and return loss 
> may be disadvantageous.
> 3. None of our suppliers have demonstrated anything else than print side 
> up.
>
> E.g. Anaren, one of our good sources
>
> http://www.anaren.com/content/File/AnarenCeramicsDesignGuide.pdf
>
> Inge
>
>
> ----- Original Message ----- 
> From: "Leland Woodall" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Thursday, July 31, 2008 12:11 PM
> Subject: Re: [TN] Repair Need for Inverted Chip Resistors
>
>
> Dewey and others,
>
> I've been told the concern lies with the resistive element being on top
> of the component.  With it being mounted upside down, the hottest
> portion of the part when under power is in direct contact with the
> board.  Would this lead to shortened life or cause any type of a
> premature failure?
>
> Are we being over-cautious about this, or is there some truth to what
> I'm being told?
>
> Leland
>
> -----Original Message-----
> From: Whittaker, Dewey (EHCOE) [mailto:[log in to unmask]]
> Sent: Thursday, July 31, 2008 2:00 PM
> To: TechNet E-Mail Forum; Leland Woodall
> Subject: RE: [TN] Repair Need for Inverted Chip Resistors
>
> I'll try to be discreet. If there is no functional impact, then a "let
> the chips fall where they may" approach is acceptable. If the part
> markings are not visible or the vision recognition algorithm of an AOI
> machine is impaired, then they may be a problem.
> Dewey
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
> Sent: Thursday, July 31, 2008 10:12 AM
> To: [log in to unmask]
> Subject: [TN] Repair Need for Inverted Chip Resistors
>
> TechPros,
>
> Can anyone tell me if there's a reliability concern with allowing chip
> resistors to be mounted upside down?  Our current policy requires that
> we repair these, and I feel that to be unnecessary.
>
> IPC-A-610D shows this to be an acceptable condition on all classes of
> product, and our customer has no specific contractual requirement.
>
> I'd like to try to change this policy at our facility, and welcome any
> commentary you might have on the subject.
>
> Thanks in advance for your help,
>
> Leland Woodall
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2