TECHNET Archives

June 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Campbell, William (wcampbel)" <[log in to unmask]>
Date:
Tue, 26 Jun 2001 14:20:44 -0400
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Campbell, William (wcampbel)" <[log in to unmask]>
Parts/Attachments:
text/plain (121 lines)
This seems a little too obvious to not have been previously considered, but
it hasn't been mentioned yet.  Is there any possibility of the parts being
damaged during depanel?  There is a very distinctive stress crack that can
be induced from depaneling, esp with v-score.  Caps can pass initially, but
fail later as the crack grows into the metalized layers.


-----Original Message-----
From: Nicole Landreville [mailto:[log in to unmask]]
Sent: Tuesday, June 26, 2001 1:10 PM
To: [log in to unmask]
Subject: Re: [TN] Multilayer Ceramic Chip Capacitors Quality


Since Frank and Genny are interested in knowing what type of capacitors we
had encountered problem with and since I believe most of you should be aware
of the following risks: First of all, ceramic multilayers capacitors are
extremely sensitive to high heat. The heat profile temperature is specified
by each manufacturer. As you probably understand, I don't feel comfortable
revealing the manufacturer's name since, as pointed out by Steven, these
manufacturing defects might not be a problem.
We observed random issues with 10 microfarads / case 2220 / for 50 V. The
capacitors we have used often showed leakage after a certain usage.
Also, we observed very constant manufacturing issues with 22 microfarads /
case 3025 / for 50 V. Electrodes are made of silver for both types.
I suspect the reliability of these capacitors is inversely proportional to
size, value and voltage.
Hope this helps more people.
Nicole
-----Original Message-----
From: Frank Kimmey [mailto:[log in to unmask]]
Sent: Tuesday, June 26, 2001 12:14 PM
To: TechNet E-Mail Forum.; [log in to unmask]
Subject: RE: [TN] Multilayer Ceramic Chip Capacitors Quality


Hi Nicole,

Could you give a little more data?
What sizes, dielectric, values?
I have seen many cap issues related to these variables and might have some
suggestions.
Call me if I can help.
FNK

Frank N Kimmey, C.I.D.
Senior PCB Designer
Powerwave Technologies
PH. 916-941-3159
Fax 916-941-3195


-----Original Message-----
From: Nicole Landreville [mailto:[log in to unmask]]
Sent: Tuesday, June 26, 2001 8:37 AM
To: [log in to unmask]
Subject: [TN] Multilayer Ceramic Chip Capacitors Quality


Bonjour a tous!
We have found some internal manufacturing defects in some Multilayers
Ceramic Chip Capacitors. After discovering reliability problems with these
types of capacitors (extreme leakage increasing with time) we have decided
to perform a construction analysis. The type of issues found relates to
misalignment of electrodes, electrode layers varying in length, warping of
dielectric plates. Unfortunately, to be able to find these manufacturing
defect we had to do a caps microsection. Now that we know that these
capacitor are prone to manufacturing defects, I would like to know if there
is any way (processes, low cost equipment or service house) to detect these
defects without scraping or damaging the caps? Originally I was thinking
that these could be X-rayed but I am not sure that the resolution would be
sharp enough. I would really appreciate if anyone could help me with this
important problem.

Thank you and good day!

Nicole Landreville, Eng.
Electrical & Supplier QC Engineer
World Heart Corporation
Ottawa, Ontario

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2