TECHNET Archives

January 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Fawn Industries, Elm City Plant" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 6 Jan 1999 11:49:09 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (67 lines)
John, Kim

It's Tom B. again, I forgot something.

It may be a dumb question on my part, but could the part be reversed, or
polarity marking on PCB reversed?

Just a thought

Tom B.


----------
> From: John Mastorides <[log in to unmask]>
> To: [log in to unmask]
> Subject: [TN] Soldering SMT Tantalum (CWR09) Caps
> Date: Wednesday, January 06, 1999 9:02 AM
>
> We have been experiencing some shorting of surface mounted tantalum
> capacitors (CWR09) which is showing up at functional test following a
> completely automated SMT process.
>
> A profile of the reflow process indicates that temperatures are within
> manufactures recommendations for these parts.  However, there are
subsequent
> operations which could be applying excessive heat to these parts. We are
> considering hand soldering these devices just prior to final test in an
> attempt to reduce frequency of failures.
>
> We have already established that the supplied capacitors not faulty.
>
> Some concern has been voiced that hand soldering is not the recommended
> method of mounting these parts.  Is anyone out there aware of concerns
> related to the reliability of hand soldering SMT tantalum capacitors?
>
> Any other recommendations?
>
> Kim O'Haver
> 813 972-6574
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2