Parash,
What flux technology are you using? For low solids fluxes (no cleans) it is
highly recommended. The deposition is more controlled and you actually put
on less flux than a foam fluxer, which is especially useful for water soluble
fluxes. There are several varieties out there. I suggest you consider the
precision flux dispenser, based on the same technology as ink-jet printers,
produced by Precision Dispensing Systems. I can furnish you more info if
desired.
Doug Pauls
[log in to unmask]
|
|
|