Parash,
What flux technology are you using?  For low solids fluxes (no cleans) it is
highly recommended.  The deposition is more controlled and you actually put
on less flux than a foam fluxer, which is especially useful for water soluble
fluxes.  There are several varieties out there.  I suggest you consider the
precision flux dispenser, based on the same technology as ink-jet printers,
produced by Precision Dispensing Systems.  I can furnish you more info if
desired.

Doug Pauls
[log in to unmask]