In a message dated 5/19/2006 6:09:56 AM Eastern Daylight Time,
[log in to unmask] writes:
How is the plating process done in PCB fabrication ? pls help me to
understand
Suganthi,
I am afraid that more than one metal is plated in PCB fabrication - copper,
nickel, tin, silver, gold, solder eutectic. And worse, there are three ways
to plate - electrodeposition with DC current, electroless with chemical
reduction, and immersion with metallic replacement.
We need for you to be a bit more specific as to the metal because several of
these can be deposited by more than one technology, above. Are you talking
about the copper in the through holes in the board?
Denny Fritz
MacDermid, Inc.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|