TECHNET Archives

July 2015

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 23 Jul 2015 14:46:06 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Mumtaz Bora <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Mumtaz Bora <[log in to unmask]>
Parts/Attachments:
text/plain (15 lines)
Dear All, Good Morning,   Looking for some knowledge base  on soldering NiPdAu finished components with low melt solder such as Sn42.0Bi57.6Ag0.4 to avoid wetting issues on a heavy copper plane board. Any insight and advise will be appreciated.

Thank-you
Mumtaz
858-795-0112
Peregrine  Semiconductor


CONFIDENTIALITY NOTE: The information transmitted, including attachments, is intended only for the person(s) or entity to which it is addressed and may contain confidential and/or privileged material. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited. If you received this in error, please contact the sender and destroy any copies of this information.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2