TECHNET Archives

December 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Bev Christian <[log in to unmask]>
Date:
Wed, 31 Dec 1997 23:24:28 -0500
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Bev Christian <[log in to unmask]>
Parts/Attachments:
text/plain (56 lines)
Werner and all,
Does anyone know if the ultrasonic methods for delamination detection in
components are powerful/sensitive enough to look through BGAs to find
either gross opens and/or hairline cracks in the BGA solder joints ?

Bev Christian
Nortel

>----------
>From:  Engelmaier[SMTP:[log in to unmask]]
>Sent:  Wednesday, December 31, 1997 5:39 PM
>To:    [log in to unmask]
>Subject:       Re: [TN] Crack detection under BGA?
>
>Hi Kevin,
>The only way you have a chance of finding cracked solder joints in product
>with BGAs is to functionally test while subjecting your assemblies to
>vibration. This gives you a chance of finding fully fractured solder joints,
>as well as use the vibration as a screening test for latent defects. However,
>with BGAs, I am not certain that even this method is 100% effective.
>
>Werner Engelmaier
>Engelmaier Associates, L.C.
>Electronic Packaging, Interconnection and Reliability Consulting
>7 Jasmine Run
>Ormond Beach, FL  32174  USA
>Phone: 904-437-8747, Fax: 904-437-8737
>E-mail: [log in to unmask]
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2