TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Mon, 14 Jul 2008 13:18:09 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Scott Gold <[log in to unmask]>
Subject:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="windows-1252"
From:
Scott Gold <[log in to unmask]>
Parts/Attachments:
text/plain (29 lines)
Hello.  New to the list and wedgebonding.  Searched the archives.  I saw 
posts about bonding to plated pads on boards, but saw nothing on using or 
bondability with plated wires.

I must avoid any oxidation on the wires.  I'm trying to find out successes, 
feasability and wire suppliers for plated aluminum wire.  Gold plating is the best 
for the outer coating for me.  From what I've read its actually 150 microinches 
Ni over 5-8 microinches of Au. Also from what i've read, the nickel is doing the 
actual bonding.

The wire is .012" or 305 um diameter. Pure gold it out of the question! :)

The bonding surface is copper etched PCB, or sometimes gold plated brass.  
Both proven to bond well with pur AL wire.

Thank you!

--Scott

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2