TECHNET Archives

April 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 26 Apr 2012 17:19:31 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (125 lines)
Hi All,

Thanks to all who have responded.  Perhaps I should add that this is a 
12-layer PCB, and the 2 oz Copper layer will be used for Power/Ground 
only.  The signal layers will be 1/2 oz thick.


Regards
Ravinder Ajmani
Principal HW Engineer, Signal Integrity / EMI
HGST, a Western Digital company
[log in to unmask]







"Lehmicke, Michael" <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
04/26/2012 02:57 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Lehmicke, Michael"     <[log in to unmask]>


To
<[log in to unmask]>
cc

Subject
Re: [TN] Core with uneven Copper foil thickness






Ravinder;

Although uneven copper thicknesses on a core are more common that one 
would expect, 1/2 oz. versus 2 oz. can cause some issues during the 
etching process, depending on trace pitch and tolerances. One would need 
to see the gerber files to determine if it would be an issue.

There are ways to get around this issue on Multilayer flex, but if this is 
just a double layer flex it has to be addressed. There are techniques, 
using a combination of additive/subtractive processes, to build up 
thickness during processing on just one side. Again, the trace widths and 
tolerances can influence this type of processing.

Mike Lehmicke
Molex Copper Flex products
22 Empire Drive
St. Paul, MN 55103
651-846-7728
[log in to unmask]




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of 
[log in to unmask]
Sent: Thursday, April 26, 2012 4:40 PM
To: [log in to unmask]
Subject: [TN] Core with uneven Copper foil thickness

Hi,

We are considering a layer stackup which uses Cores with uneven Copper
foil thickness.  Copper on one side is 1/2 oz and on the other side is 2
oz.  Apart from the availability/cost  considerations are there other
issues with using such a Core.

I will appreciate the opinions of experts on this.

Thanks.


Regards
Ravinder Ajmani
Principal HW Engineer, Signal Integrity / EMI
HGST, a Western Digital company
[log in to unmask]





______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________




CONFIDENTIALITY NOTICE: This message (including any attachments) may 
contain Molex confidential information, protected by law. If this message 
is confidential, forwarding it to individuals, other than those with a 
need to know, without the permission of the sender, is prohibited.

This message is also intended for a specific individual. If you are not 
the intended recipient, you should delete this message and are hereby 
notified that any disclosure, copying, or distribution of this message or 
taking of any action based upon it, is strictly prohibited.

English | Chinese | Japanese
www.molex.com/confidentiality.html


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2