What about partially filled PTH (with leads) and PTV. Any evidence that
this reduced reliability?
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
> Sent: Tuesday, October 01, 2002 12:28 PM
> To: [log in to unmask]
> Subject: Re: [TN] PCB design with mask over vias.
>
>
> Hi Rick,
> I have seen no evidence, nor do physics-of-failure
> considerations suggest there should be any, that there is an
> "increase in PTV barrel strength by filling the hole with
> solder." PTV interconnect structures can suffer 2 major
> failure modes: (1) barrel fracture, and (2) inner-layer
> separation [ILS]. Barrel fracture: I have seen no evidence,
> nor do physics-of-failure considerations suggest there should
> be any, that there is an "increase in PTV barrel strength by
> filling the hole with solder" regarding this failure mode.
> ILS: Filling the PTV barrel does strengthen the PTV barrel
> radially--it thus can resist the compressive loads from the
> resin thermal expansion trying to collapse the barrel. There
> is both experimental evidence and analytical reasons;
> however, I have not seen an analysis yet quantifying this effect.
>
> Werner Engelmaier
> Engelmaier Associates, L.C.
> Electronic Packaging, Interconnection and Reliability
> Consulting 7 Jasmine Run Ormond Beach, FL 32174 USA
> Phone: 904-437-8747, Fax: 904-437-8737
> E-mail: [log in to unmask], Website: www.engelmaier.com
>
> --------------------------------------------------------------
> -------------------
> Technet Mail List provided as a free service by IPC using
> LISTSERV 1.8e To unsubscribe, send a message to
> [log in to unmask] with following text in the BODY (NOT the
> subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE
> mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/html/forum.htm for
> additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
> --------------------------------------------------------------
> -------------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|