Dave,
Are you using a NoClean or OA chemistry?
If you are using NoClean and can change to OA, that might help.
If you aren't using Nitrogen in your reflow oven, you may want to try using it.
Lastly, what does your reflow profile look like? More specifically, How long
are you soaking/preheating and in what temperature range?
-Carrie
-----Original Message-----
From: Dave Hornback [mailto:[log in to unmask]]
Sent: Thursday, November 21, 2002 11:28 AM
To: [log in to unmask]
Subject: [TN] SMT component oxidation
Hello TechNet folks, I need a little help. We have an SMT RF duplexor that
has a ~20% yield hit due to bad wetting under the component, we suspect
they have slight oxidation. Because it is an RF component the solder
process must be very consistent. On the units that fail we can remove the
component, add a little flux, then reflow the same component back onto the
board. This fixes nearly all the failures. The parts are in tape and reel
and are not convenient to pre-tin.
One of our mfg folks suggested we add a little liquid flux on top of the
paste immediately after screening. This is the last build of this product,
just 75 units, so we don't want to re-engineer the entire process. Has
anyone tried something like this? I'm a little nervous to introduce a
science project at this stage.
Any advice? Thanks, Dave
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|