Leif,
Plugging of vias is covered by IPC 4761 "Design Guide for Protection of Printed Board Via Structures".
Flush via plugging is possible, but is generally achieved with a via fill that can be planarized after application vs. a via plugging with soldermask.
-----Original Message-----
From: Leif Erik Laerum [mailto:[log in to unmask]]
Sent: Monday, September 28, 2009 12:03 PM
To: [log in to unmask]
Subject: [TN] Plug vias first or second.
Technetters,
We have a problem with certain PCBs where plugged vias have a solder
mask "mound" that creates a coplanarity issues and also causes the
screen to be elevated. The elevated screen results in excessive solder
deposit and massive amount of shorts for the finest pitch parts. We
believe the root cause is the practice of plugging the vias with solder
mask after they have been covered. This seems to result in these mounds
instead of a planar surface. From what we understand, this is the
preferred order of the two steps by PCB vendors.
Why is this preferred?
Is there a IPC spec that covers this issue?
Is it reasonable to specify that the plugging must result in no mounds
and 0 elevation of the vias?
Is there a particular process weakness from the PCB vendors that causes
this defect?
Thank you.
--
Leif Erik Laerum
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|