Re: Soldermask thickness causing 0402 tombstones?
From:
Brian Chandler <
[log in to unmask]
>
Reply To:
TechNet E-Mail Forum <
[log in to unmask]
>, Brian Chandler <
[log in to unmask]
>
Date:
Mon, 15 Jul 2013 07:12:08 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain
(2 lines)
Yes, the root cause in my case was debris under the solder mask causing high spots.