TECHNET Archives

September 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Ken Bloomquist <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ken Bloomquist <[log in to unmask]>
Date:
Wed, 3 Sep 2008 09:08:56 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (127 lines)
It was static dissipative!

Thinking a little bit more about this I believe that metalized static
dissipative bags are a sandwich of materials. Isn't the inside layer of a
static dissipative bag basically nonconductive plastic similar to Jon's pink
bubble wrap?

KennyB

-----Original Message-----
From: Roberts, Jon [mailto:[log in to unmask]] 
Sent: Wednesday, September 03, 2008 8:46 AM
To: TechNet E-Mail Forum; Ken Bloomquist
Subject: RE: [TN] ANTISTATIC MATERIAL QUESTION

KennyB, was the ESD bag an antistatic or static dissipative?  Thanks,
Jon 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
Sent: Wednesday, September 03, 2008 10:36 AM
To: [log in to unmask]
Subject: Re: [TN] ANTISTATIC MATERIAL QUESTION

Hi Jon,

I'm not sure what the drying time is on the AR that you are using but I
know
with the UR we use takes about a week to fully dry. We experienced a
situation where we were having some boards built and coated in Mexico.
The
boards were put into ESD bags after a couple of days and shipped to our
facility. A combination of not being fully dried and sitting in a hot
truck
in the Mexican sun at the border cause the bags to stick to the coating.
When we tried to remove the bags they had to be cut away they were stuck
so
badly.

I guess what I'm saying is to make sure that they are fully cured before
putting them into the "proper" ESD packaging.

KennyB

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]] 
Sent: Wednesday, September 03, 2008 8:05 AM
To: [log in to unmask]
Subject: Re: [TN] ANTISTATIC MATERIAL QUESTION

Date:    Tue, 2 Sep 2008 10:43:10 -0500
From:    "Roberts, Jon" <[log in to unmask]>
Subject: ANTISTATIC MATERIAL QUESTION

We have been noticing if bubble wrap is allowed to come in direct
contact with a circuit card assembly (non ESD and ESD) sensitive that
the bubble wrap leaves impression in the AR coating.  Do know if the
resulting impression is related to uncured coating or reaction of the
bubble wrap material?  Thanks for any information, Jon



Jon,

Not to be a stickler on coating questions, but there is no such thing as
uncured AR coating. Because the coating is lacquer, it doesn't cure, it
only
dries. The solvents in which the acrylic resin is dissolved leave the
coating and all that is left is the plastic.?That plastic does not
cross-link, so it?can be redissolved at will, and that's why AR is the
strippable coating that it is.?Insufficient drying?could?contibute to
the
condition you describe.?In our experience?we believe that plasticizers
from
the bubble wrap (notoriously oily, nasty stuff, it even seems like the
antistatic is worse) are actually redissolving the coating in areas of
contact. This would be more noticeable if the coating were not
completely
dry, since it's already somewhat melted. In any case, our solution is
not to
let the bubble wrap come into direct contact with any type AR coating.

Mike Moninger
Thermospray Company Inc.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

This communication is intended only for use by the addressee(s) named herein
and may contain business confidential and/or legally privileged information.
If you are not the intended recipient of this e-mail, you are hereby
notified that any dissemination, distribution, disclosure or copying of this
e-mail and its contents is strictly prohibited. If you have received this
e-mail in error, kindly notify the sender by replying to this message. In
addition, please permanently delete the message and any attachments without
copying or disclosing the contents. Thank you for your cooperation.

THIS DOCUMENT AND/OR SHIPMENT MAY CONTAIN COMMODITY ITEMS, SOFTWARE OR
TECHNICAL DATA THAT IS CONTROLLED BY U.S. EXPORT LAW, AND MAY NOT BE
EXPORTED OUTSIDE THE UNITED STATES OR TO NON U.S. PERSONS WITHOUT THE
APPROPRIATE EXPORT LICENSE FROM EITHER THE U.S. DEPARTMENT OF STATE OR
DEPARTMENT OF COMMERCE.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2