"Stadem, Richard D." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard D.
Date:
Tue, 13 Nov 2007 10:01:32 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (74 lines)
I have to agree with Liang. If the printed solder paste melted at all, some of the solder should have wetted to the board pads.
However, solder follows the heat. If the pad temperature is too low, but the component is quite hot, theoretically the molten solder could wick up onto the component terminations. However, I really doubt that is the case, because apparently there is enough heat to get the solder paste to melt, and that should be hot enough for the solder to wet to the pads as well. Total nonwetting of the solder to the pads indicates a solderability issue with those pads.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Liang Yin
Sent: Friday, November 09, 2007 10:59 AM
To: [log in to unmask]
Subject: Re: [TN] non wetting

Lon,

What your PCB producer told you does not make sense. 

Although the tin-lead alloy might have different wetting performance on flash gold pads, it should not have non-wetting in any event. If the flash gold is still there after soldering process, you have solderability problem with the boards. X-ray inspection is not a solderability test. 

Liang Yin
Process Research Engineer

Unovis Solutions 



> Date: Fri, 9 Nov 2007 16:23:00 +0100
> From: [log in to unmask]
> Subject: [TN] non wetting
> To: [log in to unmask]
> 
> Dear Technetters,
> 
> We had two boards out of 25 with a nonwetting problem. After reflow there was no solder on the flashgolden pads. Instead all the solder had gone to the leads of the 0805 capacitor.
> 
> Our pcb producer comes with the following conclusion:
> 
>  	"Our Q-dept. just informed me that they did x-ray inspection of the 2  boards you sent us back recently. Apparently 	there have been components used which contain up to 20% lead. During reflow-soldering the tin-lead on those 	components will melt first and absorb all the solder paste even before the tin which is included in the solder paste 	will melt. A golden flashgold pad without any tin will be the result. The tin will accumulate on the components and 	create those solder-balls instead. 
> 
> 	In a second test we did lead-free soldering  on the side which contains no components. The two PCBs showed excellent 	tin-wetting on this side. All pads - big and small ones - are nicely covered with tin. So basically we will reject 	any complaint - the boards are ok."
> 
> 
> Does this make sense?
> 
> Regards,
> 
> Lon Weffers
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
> unsubscribe, send a message to [log in to unmask] with following text in 
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET 
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the 
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the 
> archives of previous posts at: http://listserv.ipc.org/archives Please 
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at 
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------

_________________________________________________________________
Boo! Scare away worms, viruses and so much more! Try Windows Live OneCare!
http://onecare.live.com/standard/en-us/purchase/trial.aspx?s_cid=wl_hotmailnews
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2