Steve
We use customer specs when applicable, but we use IPC 6012 Class II as a
default for when a customer spec is not available or does not cover an
issue. So there would be no adder. I would think that would be true at
most places. A lot of our customer specs start with IPC 6012 Class2 (or 3),
then note exceptions to it.
Mike McMaster
RF Product Engineer
Merix Corporation
503-992-4263
> ----------
> From: Steve Gregory[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;[log in to unmask]
> Sent: Monday, September 15, 2003 8:11 AM
> To: [log in to unmask]
> Subject: [TN] Building Fabs to IPC-6012 spec's...
>
> Hi All!
>
> Just a general question; how much of a cost adder would be incurred
> building
> Class-2 fabs that comply with all the IPC-6012 specifications?
>
> Thanks!
>
> -Steve Gregory-
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|