I forgot to mention, that I have seen how the solder balls elongate during
pull or prey test. They change from a flatted ball to a barrel. That means
that the volume between the BGA and the board nearly doubles! I was very
surprised. Didn't think solder was like chewing gum. Does the coating or
underfiller really expand that much?
I'm very interested in this, as we produce boards with a lot of largest
available BGAs.
Inge
PS. Will see if I still have the amazing photos from the test.
----- Original Message -----
From: "Inge" <[log in to unmask]>
To: "TechNet E-Mail Forum" <[log in to unmask]>; <[log in to unmask]>
Sent: Monday, November 30, 2009 10:15 PM
Subject: Re: [TN] BGAs & Conformal Coating
> Doug,
>
> how can that be possible? When temperature rises, the coating ought to
> soften and should expand even horisontally, and when at lower
> temperatures, the coating should crimp. The only way I can see is if you
> have the situation of a closed in liquid, which one cannot be compressed.
> BGAs use to be very hard to rip from the board. I measured some 350 kg
> force necessary to pull off a very large BGA.
>
> Inge
>
>
>
> ----- Original Message -----
> From: "Douglas Pauls" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Monday, November 30, 2009 2:29 PM
> Subject: Re: [TN] BGAs & Conformal Coating
>
>
> Good morning Juan,
> I suspect that Xilinx wants you do do a thermal cycle study on solder
> joint reliability when conformal coating gets under the BGA. The stresses
> brought about by a mismatches in the coefficient of thermal expansion
> (CTE) can rip a BGA off the board and can severely deform the balls.
> Hillman and I did such a study here a few years ago. I can share a few
> pictures of what happens, if Steve Gregory would be kind enough to forward
> his present e-mail address for the photos. Not sure I have the right one.
>
> Doug Pauls
>
>
>
> "Juan T. Marugán" <[log in to unmask]>
> Sent by: TechNet <[log in to unmask]>
> 11/26/2009 11:53 AM
> Please respond to
> TechNet E-Mail Forum <[log in to unmask]>; Please respond to
> "Juan T. Marugán" <[log in to unmask]>
>
>
> To
> [log in to unmask]
> cc
>
> Subject
> [TN] BGAs & Conformal Coating
>
>
>
>
>
>
> Hi,
>
> I've read in a Xilinx guide that: "Xilinx has no experience or reliability
> data on
> flip-chip BGA packages on board after exposure to conformal coating. It is
>
> recommended that the end-user should characterize the board level
> reliability
> performance of Xilinx packages before production use."
>
> Does anybody know any infomation or study related with this topic?
>
> Thank you.
>
> Juan T. Marugán
> Indra Sistemas SA
> Espańa
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|