TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Colin Weber <[log in to unmask]>
Date:
Wed, 1 Jul 1998 15:29:49 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Jerry Cupples <[log in to unmask]>
Subject:
From:
Jerry Cupples <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (47 lines)
Colin Weber said:

>I have been reviewing comments from past emails to the Technet forum
>w.r.t. gold finishes on edge connectors.
>
>I have concluded I should not require a nickel barrier for my application.
>This could be qualified by noting the board will not be used in harsh
>environments or be inserted more than several times in it's lifetime.

Hang on a bit; before you conclude here's another comment: copper will
rapidly diffuse into the porous gold. The nickel barrier is universally
used between Cu and Au, and without it you will soon see a very ugly and
high resistance dark color on the thin Au plating typical of board
contacts. It's not simply a matter of hardness or wear resistance. Copper
oxides will make that edge connector a no-connect at logic voltages.

>However I am still left wondering about the thickness of the hard gold
>finish. In the past I have specified, for Class3, 1.3um. However, the
>product shall be used in a class 2 environment.
>Are there any disadvantages in using 1.3um (particularly since the IPC
>standards state 0.8um for class 2), apart from cost?

No. Bellcore/ATT used to require 50 uin Au, they still show it as a
"preferred" finish. To some extent, the additional thickness is a safety
factor because of the known porosity of Au electroplate finishes.


regards,


Jerry Cupples
Interphase Corporation
Dallas, TX USA
http://www.iphase.com

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2