Steve,
There is always a tiny peak if oxygen in a spectrum collected from a solder joint ad the surface us oxidized. If you see a large peak of O then I'd prefer to see the actual spectrum.
Regards,
Vladimir Igoshev
SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7
Scarborough, ON M1R 5G1
Phone: 647-495-8727
Cell: 416-899-1882
[log in to unmask]
www.sentec.ca
Original Message
From: Steven Kelly
Sent: Friday, May 23, 2014 9:55 AM
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: [TN] SEM/EDX ANALYSIS
Hi All,
Can someone explain to me why in a SEM/EDX analysis of a solder joint there would be Oxygen?
Thanks Steve Kelly
If the recipient to whom this e-mail is sent has an NDA with PFC Flexible Circuits Limited this e-mail is considered confidential and is subject to any NDA agreements between the respective parties.
See PFC on "How its' Made" April 17th on the Discovery Channel
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|