Dear Technet,
For a small shop without automation or ppr, what is a standard time
acceptable to
plate moderate to low difficulty double- sided boards to 1 mil with a
standard acid copper plating solution?
Our vendor can offer us a different brightner system, etc., I was just
looking for a
norm. We can make adjustments to speed our cycles, but we give up even
distribution.
Thanks,
Green
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|