I did not see any one mention the fact that the leads of this component are
passing through a seal that is intended to keep an electrolyte inside the
component. Stressing the seal in this manner is unacceptable. It will very
likely cause the component to fail prematurely.
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Andre Leclair
> Sent: Wednesday, December 12, 2001 8:26 AM
> To: [log in to unmask]
> Subject: [TN] To form or not to Form
>
>
> Hi all
> I hope this gets some good advice.
>
> I have a customer who is requiring the placement of an electrolitic cap
> that has a lead spacing of 0.140" and the PCB has 0.100". They
> do not want
> the leads formed, they want the part flat to the board. In doing this, am
> I opening myself up to stress induced failures of the component.
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following
> message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|