TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"COOKE, ROBERT W. (JSC-NX) (WGI)" <[log in to unmask]>
Date:
Fri, 27 May 2005 09:13:00 -0500
MIME-Version:
1.0
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "COOKE, ROBERT W. (JSC-NX) (WGI)" <[log in to unmask]>
Parts/Attachments:
text/plain (70 lines)
Rich,

Electroless nickel (EN) plating is generally solderable until the phosphor
content in the plating exceeds 5-7 percent. (H. Manko, Solders and
Solderability)

However, solderability may be adversely affected in EN platings with as low
as 3.5% percent phosphor content if the plating has been subjected to heat
treating. (B. Dunn, Metallurgical Assessment of Spacecraft Parts, Materials
and Processes)

Tin-lead solder tinning of electroless nickel plated copper wire can be
accomplished successfully at +725-750F with RMA or RA flux.

Bob


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Friday, May 27, 2005 8:11 AM
To: [log in to unmask]
Subject: [TN] Solderablity of ElectrolessNickel

I'm trying to clearly confirm the level of phosphorus at which the
solderability of electroless nickel starts to be severely reduced.

Traditionally, I always thought it was 5%. I colleague of mine claims
that he's got a paper from 89' at the "Electroless Ni Conference" that
states that up to 3% is no problem.  I do recall seeing an article last
year where  6 to 8% seems to be the preferred maximum .

Any thoughts on what the appropriate level should be, and/or the
mechanism of why it is it degrades solderablity would be truly
appreciated.

Rich K - KEDS










---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2